7xxx Series · Temper T7451 · AMS 4050 / ASTM B209 / EN AW-7050

7050-T7451 Aluminum — Properties, Weight Calculator & Engineering Datasheet

Thick-plate aerospace structural alloy (Al-Zn-Mg-Cu-Zr). Overaged T7451 temper eliminates Stress Corrosion Cracking (SCC) while preserving high fracture toughness in 50–150 mm hog-out plates.

Specific Strength (Rp0.2 / ρ)
165.7 kN·m/kg
True ρ = 2.83 g/cm³

Density (ρ)

2.83 g/cm³

2830 kg/m³ · 0.1022 lb/in³

Yield (Rp0.2)

469 MPa

68 ksi (0.2% offset)

Tensile (Rm)

524 MPa

76 ksi ultimate

Shear Strength (τu)

303 MPa

Ultimate shear

Fatigue Limit

165 MPa

5×10⁸ cycles RR Moore

Bearing Yield

710 MPa

e/D = 2.0 pin/rivet

Elongation (A)

11%

Min bend R ≈ 6×t

Modulus (E)

71.7 GPa

Shear G ≈ 27 GPa

Hardness

140 HB

Temper T7451

α Thermal Exp.

23.5×10⁻⁶/K

20–100 °C linear

k Thermal Cond.

157 W/m·K

488 – 629 °C

Elec. Cond.

41% IACS

CNC Vc ≈ 420 m/min

Interactive Engineering Workbench · 7050-T7451 Aluminum (AMS 4050 / ASTM B209 / EN AW-7050)

7050-T7451 Aluminum Live Calculator & Design Verification Suite

True Mass (2.83 g/cm³)
8.49 kg
18.72 lb (8.490 kg/pc)
If Assumed ρ = 2.70 g/cm³
8.10 kg
Δ = +0.39 kg (+4.81%)
Estimated Material Cost
$57.73
Vol: 3000 cm³ · A: 3000 mm²
Engineering Mass Traceability Note

7050-T7451 Aluminum contains alloying elements (7xxx series) that shift its density to 2.83 g/cm³ (2830 kg/m³). On a 1-piece batch, generic 2.70 g/cm³ calculators miscalculate shipping and structural mass by 390 grams.

Chemical Composition Limits (wt% per AMS 4050 / ASTM B209 / EN AW-7050)

Nominal elemental mass fractions governing density (2.83 g/cm³), precipitation hardening, and weldability.

EN 573-3 / AA Registered Limits
Al
87.3–90.3%
Cu
2.0–2.6%
Mg
1.9–2.6%
Mn
≤ 0.10%
Si
≤ 0.12%
Zn
5.7–6.7%
Cr
≤ 0.04%
Fe
≤ 0.15%

Standard Nominal Density vs Generic 2.70 g/cm³ Baseline

Nominal standard density for 7050-T7451 Aluminum is 2.83 g/cm³ (2830 kg/m³ per AMS 4050 / ASTM B209 / EN AW-7050). Assuming a generic 2.70 g/cm³ aluminum density introduces a +4.81% mass discrepancy across BOM, structural payload, and freight logistics calculations.

Normative Specification vs Lot Inspection: Values shown are normative nominal design baselines per AMS 4050 / ASTM B209 / EN AW-7050 and EN 573-3. Lot-specific physical properties and chemical compositions are documented on manufacturer Mill Test Certificates (EN 10204 Type 3.1 / 3.2). Mechanical strength values represent standard minimum guarantees for extruded profiles (typically wall thickness t ≤ 5 mm); thicker gauges, plate products (EN 485), and specific tempers follow dedicated standard sub-clauses.

1 m² × 10 mm plate (True ρ = 2.83)

28.30 kg

Same plate if assumed ρ = 2.70

27.00 kg

Mass Discrepancy per Plate

+1.30 kg (2.87 lb)

Weldability (EN 1999 / AWS)

Poor

Join via mechanical fasteners (Hi-Lok, 2117-T4 AD rivets, or VDI 2230 bolts).

CNC Machinability

Excellent

Recommended 3-flute carbide Vc ≈ 420 m/min.

Corrosion & Anodizing

Good

Melting range: 488 – 629 °C.

Typical Industrial Applications

  • • Monolithic CNC wing bulkheads & fuselage frames
  • • Fighter jet structural ribs
  • • High-precision injection molds
  • • Semiconductor vacuum chambers

Engineering Pitfalls & Design Warnings

  • ⚠ Highest common aluminum density (2.83 g/cm³ — +4.8% heavier than 2.70)
  • ⚠ Never fusion weld; join with aerospace interference-fit fasteners

Compare 7050-T7451 Aluminum & Explore All Aluminum Alloys

Methodology Tier 1 Normative Reference: AMS 4050 / ASTM B209 / EN AW-7050 / EN 573-3 / EN 485-2 / MMPDS. Values are typical handbook figures for temper T7451.