6xxx Series · Temper T6 · EN 755 / EN 485 / EN AW-6082

6082-T6 Aluminum — Properties, Weight Calculator & Engineering Datasheet

Primary European structural Al-Si-Mg-Mn alloy (Eurocode 9). Manganese refines grain structure for superior toughness in bridges, trusses, and cranes.

Specific Strength (Rp0.2 / ρ)
95.9 kN·m/kg
True ρ = 2.71 g/cm³

Density (ρ)

2.71 g/cm³

2710 kg/m³ · 0.0979 lb/in³

Yield (Rp0.2)

260 MPa

38 ksi (0.2% offset)

Tensile (Rm)

310 MPa

45 ksi ultimate

Shear Strength (τu)

190 MPa

Ultimate shear

Fatigue Limit

95 MPa

5×10⁸ cycles RR Moore

Bearing Yield

410 MPa

e/D = 2.0 pin/rivet

Elongation (A)

10%

Min bend R ≈ 3×t

Modulus (E)

70 GPa

Shear G ≈ 27 GPa

Hardness

95 HB

Temper T6

α Thermal Exp.

24.0×10⁻⁶/K

20–100 °C linear

k Thermal Cond.

180 W/m·K

575 – 650 °C

Elec. Cond.

44% IACS

CNC Vc ≈ 460 m/min

Interactive Engineering Workbench · 6082-T6 Aluminum (EN 755 / EN 485 / EN AW-6082)

6082-T6 Aluminum Live Calculator & Design Verification Suite

True Mass (2.71 g/cm³)
8.13 kg
17.92 lb (8.130 kg/pc)
If Assumed ρ = 2.70 g/cm³
8.10 kg
Δ = +0.03 kg (+0.37%)
Estimated Material Cost
$55.28
Vol: 3000 cm³ · A: 3000 mm²
Engineering Mass Traceability Note

6082-T6 Aluminum contains alloying elements (6xxx series) that shift its density to 2.71 g/cm³ (2710 kg/m³). On a 1-piece batch, generic 2.70 g/cm³ calculators miscalculate shipping and structural mass by 30 grams.

Chemical Composition Limits (wt% per EN 755 / EN 485 / EN AW-6082)

Nominal elemental mass fractions governing density (2.71 g/cm³), precipitation hardening, and weldability.

EN 573-3 / AA Registered Limits
Al
95.2–98.3%
Cu
≤ 0.10%
Mg
0.6–1.2%
Mn
0.40–1.0%
Si
0.7–1.3%
Zn
≤ 0.20%
Cr
≤ 0.25%
Fe
≤ 0.50%

Standard Nominal Density vs Generic 2.70 g/cm³ Baseline

Nominal standard density for 6082-T6 Aluminum is 2.71 g/cm³ (2710 kg/m³ per EN 755 / EN 485 / EN AW-6082). Assuming a generic 2.70 g/cm³ aluminum density introduces a +0.37% mass discrepancy across BOM, structural payload, and freight logistics calculations.

Normative Specification vs Lot Inspection: Values shown are normative nominal design baselines per EN 755 / EN 485 / EN AW-6082 and EN 573-3. Lot-specific physical properties and chemical compositions are documented on manufacturer Mill Test Certificates (EN 10204 Type 3.1 / 3.2). Mechanical strength values represent standard minimum guarantees for extruded profiles (typically wall thickness t ≤ 5 mm); thicker gauges, plate products (EN 485), and specific tempers follow dedicated standard sub-clauses.

1 m² × 10 mm plate (True ρ = 2.71)

27.10 kg

Same plate if assumed ρ = 2.70

27.00 kg

Mass Discrepancy per Plate

+0.10 kg (0.22 lb)

Weldability (EN 1999 / AWS)

Good

TIG/MIG weldable using ER4043 or ER5356 filler wire.

CNC Machinability

Good

Recommended 3-flute carbide Vc ≈ 460 m/min.

Corrosion & Anodizing

Good

Melting range: 575 – 650 °C.

Typical Industrial Applications

  • • Stage trusses & pedestrian bridges
  • • Crane booms & transport chassis
  • • CNC machined tooling plates
  • • Offshore helidecks

Engineering Pitfalls & Design Warnings

  • ⚠ Weld HAZ loses T6 strength (use ER5356 for shear strength or ER4043 for crack resistance)
  • ⚠ Thin walls (<2 mm) are harder to extrude than 6060/6005A

Compare 6082-T6 Aluminum & Explore All Aluminum Alloys

Methodology Tier 1 Normative Reference: EN 755 / EN 485 / EN AW-6082 / EN 573-3 / EN 485-2 / MMPDS. Values are typical handbook figures for temper T6.