6xxx Series · Temper T5 · ASTM B221 / EN AW-6063

6063-T5 Aluminum — Properties, Weight Calculator & Engineering Datasheet

Architectural extrusion and thermal management specialist. Smoother surface finish and 25% higher thermal conductivity than 6061-T6.

Specific Strength (Rp0.2 / ρ)
53.7 kN·m/kg
True ρ = 2.70 g/cm³

Density (ρ)

2.70 g/cm³

2700 kg/m³ · 0.0975 lb/in³

Yield (Rp0.2)

145 MPa

21 ksi (0.2% offset)

Tensile (Rm)

185 MPa

27 ksi ultimate

Shear Strength (τu)

117 MPa

Ultimate shear

Fatigue Limit

69 MPa

5×10⁸ cycles RR Moore

Bearing Yield

235 MPa

e/D = 2.0 pin/rivet

Elongation (A)

8%

Min bend R ≈ 2×t

Modulus (E)

68.9 GPa

Shear G ≈ 27 GPa

Hardness

60 HB

Temper T5

α Thermal Exp.

23.4×10⁻⁶/K

20–100 °C linear

k Thermal Cond.

209 W/m·K

615 – 654 °C

Elec. Cond.

55% IACS

CNC Vc ≈ 450 m/min

Interactive Engineering Workbench · 6063-T5 Aluminum (ASTM B221 / EN AW-6063)

6063-T5 Aluminum Live Calculator & Design Verification Suite

True Mass (2.70 g/cm³)
8.10 kg
17.86 lb (8.100 kg/pc)
If Assumed ρ = 2.70 g/cm³
8.10 kg
Δ = +0.00 kg (+0.00%)
Estimated Material Cost
$55.08
Vol: 3000 cm³ · A: 3000 mm²
Engineering Mass Traceability Note

6063-T5 Aluminum contains alloying elements (6xxx series) that shift its density to 2.70 g/cm³ (2700 kg/m³). On a 1-piece batch, generic 2.70 g/cm³ calculators miscalculate shipping and structural mass by 0 grams.

Chemical Composition Limits (wt% per ASTM B221 / EN AW-6063)

Nominal elemental mass fractions governing density (2.70 g/cm³), precipitation hardening, and weldability.

EN 573-3 / AA Registered Limits
Al
97.5–99.3%
Cu
≤ 0.10%
Mg
0.45–0.90%
Mn
≤ 0.10%
Si
0.20–0.60%
Zn
≤ 0.10%
Cr
≤ 0.10%
Fe
≤ 0.35%

Standard Nominal Density vs Generic 2.70 g/cm³ Baseline

Nominal standard density for 6063-T5 Aluminum is 2.70 g/cm³ (2700 kg/m³ per ASTM B221 / EN AW-6063). For 6063-T5 Aluminum, this nominal density coincides with the generic 2.70 g/cm³ baseline. However, for higher-alloyed grades (such as 6082 at 2.71 g/cm³ or 7075 at 2.81 g/cm³), true handbook values must be used to avoid mass deviations.

Normative Specification vs Lot Inspection: Values shown are normative nominal design baselines per ASTM B221 / EN AW-6063 and EN 573-3. Lot-specific physical properties and chemical compositions are documented on manufacturer Mill Test Certificates (EN 10204 Type 3.1 / 3.2). Mechanical strength values represent standard minimum guarantees for extruded profiles (typically wall thickness t ≤ 5 mm); thicker gauges, plate products (EN 485), and specific tempers follow dedicated standard sub-clauses.

1 m² × 10 mm plate (True ρ = 2.70)

27.00 kg

Same plate if assumed ρ = 2.70

27.00 kg

Mass Discrepancy per Plate

+0.00 kg (0.00 lb)

Weldability (EN 1999 / AWS)

Good

TIG/MIG weldable using ER4043 or ER5356 filler wire.

CNC Machinability

Good

Recommended 3-flute carbide Vc ≈ 450 m/min.

Corrosion & Anodizing

Excellent

Melting range: 615 – 654 °C.

Typical Industrial Applications

  • • Architectural window & curtain wall extrusions
  • • Extruded CPU/IGBT heat sinks
  • • Handrails & balustrades
  • • Pneumatic cylinder barrels

Engineering Pitfalls & Design Warnings

  • ⚠ Do not specify 6063-T5 where 6061-T6 yield strength (275 MPa) is required
  • ⚠ T5 press-quenched temper is ~20% weaker than T6 water-quenched

Compare 6063-T5 Aluminum & Explore All Aluminum Alloys

Methodology Tier 1 Normative Reference: ASTM B221 / EN AW-6063 / EN 573-3 / EN 485-2 / MMPDS. Values are typical handbook figures for temper T5.