2xxx Series · Temper T6 · ASTM B209 / EN AW-2014A

2014-T6 Aluminum — Properties, Weight Calculator & Engineering Datasheet

High-strength aerospace and heavy-duty forging Al-Cu-Si alloy. Higher yield than 2024-T3 with density 2.80 g/cm³.

Specific Strength (Rp0.2 / ρ)
147.9 kN·m/kg
True ρ = 2.80 g/cm³

Density (ρ)

2.80 g/cm³

2800 kg/m³ · 0.1012 lb/in³

Yield (Rp0.2)

414 MPa

60 ksi (0.2% offset)

Tensile (Rm)

483 MPa

70 ksi ultimate

Shear Strength (τu)

290 MPa

Ultimate shear

Fatigue Limit

124 MPa

5×10⁸ cycles RR Moore

Bearing Yield

660 MPa

e/D = 2.0 pin/rivet

Elongation (A)

13%

Min bend R ≈ 5×t

Modulus (E)

72.4 GPa

Shear G ≈ 27 GPa

Hardness

135 HB

Temper T6

α Thermal Exp.

23.0×10⁻⁶/K

20–100 °C linear

k Thermal Cond.

154 W/m·K

507 – 638 °C

Elec. Cond.

40% IACS

CNC Vc ≈ 380 m/min

Interactive Engineering Workbench · 2014-T6 Aluminum (ASTM B209 / EN AW-2014A)

2014-T6 Aluminum Live Calculator & Design Verification Suite

True Mass (2.80 g/cm³)
8.40 kg
18.52 lb (8.400 kg/pc)
If Assumed ρ = 2.70 g/cm³
8.10 kg
Δ = +0.30 kg (+3.70%)
Estimated Material Cost
$57.12
Vol: 3000 cm³ · A: 3000 mm²
Engineering Mass Traceability Note

2014-T6 Aluminum contains alloying elements (2xxx series) that shift its density to 2.80 g/cm³ (2800 kg/m³). On a 1-piece batch, generic 2.70 g/cm³ calculators miscalculate shipping and structural mass by 300 grams.

Chemical Composition Limits (wt% per ASTM B209 / EN AW-2014A)

Nominal elemental mass fractions governing density (2.80 g/cm³), precipitation hardening, and weldability.

EN 573-3 / AA Registered Limits
Al
90.4–95.0%
Cu
3.9–5.0%
Mg
0.20–0.80%
Mn
0.40–1.2%
Si
0.50–1.2%
Zn
≤ 0.25%
Cr
≤ 0.10%
Fe
≤ 0.70%

Standard Nominal Density vs Generic 2.70 g/cm³ Baseline

Nominal standard density for 2014-T6 Aluminum is 2.80 g/cm³ (2800 kg/m³ per ASTM B209 / EN AW-2014A). Assuming a generic 2.70 g/cm³ aluminum density introduces a +3.70% mass discrepancy across BOM, structural payload, and freight logistics calculations.

Normative Specification vs Lot Inspection: Values shown are normative nominal design baselines per ASTM B209 / EN AW-2014A and EN 573-3. Lot-specific physical properties and chemical compositions are documented on manufacturer Mill Test Certificates (EN 10204 Type 3.1 / 3.2). Mechanical strength values represent standard minimum guarantees for extruded profiles (typically wall thickness t ≤ 5 mm); thicker gauges, plate products (EN 485), and specific tempers follow dedicated standard sub-clauses.

1 m² × 10 mm plate (True ρ = 2.80)

28.00 kg

Same plate if assumed ρ = 2.70

27.00 kg

Mass Discrepancy per Plate

+1.00 kg (2.20 lb)

Weldability (EN 1999 / AWS)

Poor

Join via mechanical fasteners (Hi-Lok, 2117-T4 AD rivets, or VDI 2230 bolts).

CNC Machinability

Excellent

Recommended 3-flute carbide Vc ≈ 380 m/min.

Corrosion & Anodizing

Fair

Melting range: 507 – 638 °C.

Typical Industrial Applications

  • • Aerospace primary forgings
  • • Military vehicle frames
  • • Rocket booster rings
  • • Heavy hydraulic manifolds

Engineering Pitfalls & Design Warnings

  • ⚠ Prone to hot cracking if fusion welded
  • ⚠ Requires anodizing or Alclad protection in marine/outdoor exposure

Compare 2014-T6 Aluminum & Explore All Aluminum Alloys

Methodology Tier 1 Normative Reference: ASTM B209 / EN AW-2014A / EN 573-3 / EN 485-2 / MMPDS. Values are typical handbook figures for temper T6.